| MOQ: | 100 kg |
| Harga: | Price is negotiated based on the required specifications and quantity |
| standard packaging: | Kemasan standar ekspor, atau kemasan sesuai kebutuhan |
| Delivery period: | 5-8 hari kerja, tergantung parameter yang diperlukan untuk negosiasi |
| metode pembayaran: | Ketentuan Pembayaran: Terutama T/T .. L/C, D/A, D/P, |
| Supply Capacity: | 5000 Ton per Bulan |
| Elemen | Komposisi (%) |
|---|---|
| Nikel (Ni) | Saldo |
| Besi (Cr) | 19.0 - 21.0 |
| Cobalt (Co) | 10.0 - 12.0 |
| Molybdenum (Mo) | 3.0 - 4.0 |
| Tungsten (W) | 2.0 - 3.0 |
| Titanium (Ti) | 2.0 - 2.5 |
| Aluminium (Al) | 1.0 - 1.5 |
| Karbon (C) | ≤ 0.08 |
| Silikon (Si) | ≤ 0.50 |
| Mangan (Mn) | ≤ 0.50 |
| Bor (B) | ≤ 0.01 |