| Element | Composition (%) |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 19.0 - 21.0 |
| Cobalt (Co) | 10.0 - 12.0 |
| Molybdenum (Mo) | 3.0 - 4.0 |
| Tungsten (W) | 2.0 - 3.0 |
| Titanium (Ti) | 2.0 - 2.5 |
| Aluminum (Al) | 1.0 - 1.5 |
| Carbon (C) | ≤ 0.08 |
| Silicon (Si) | ≤ 0.50 |
| Manganese (Mn) | ≤ 0.50 |