Found 46 Products For:

"stainless steel wire"

Quality Nickel Alloy X-750 | UNS N07750 | 2.4669 | Inconel X-750 factory

Nickel Alloy X-750 | UNS N07750 | 2.4669 | Inconel X-750

Nickel Alloy X-750 (UNS N07750 / 2.4669) is a precipitation-hardenable nickel-chromium alloy with high strength to 704°C, oxidation resistance to 982°C, and excellent relaxation resistance. Available in plate, round bar and wire with EN 10204 3.1 certification .
Quality Nickel Alloy 718 | UNS N07718 High-Strength Superalloy factory

Nickel Alloy 718 | UNS N07718 High-Strength Superalloy

Nickel Alloy 718 (UNS N07718 / 2.4668) is an age-hardenable nickel-chromium-iron superalloy with high tensile strength up to 185 ksi, creep resistance to 700°C, and good weldability. Available in plate, sheet, round bar, and forgings with PMI and EN 10204 3.1 certification.
Quality Nickel Alloy 800HT | UNS N08811 | 1.4959 | Incoloy 800HT factory

Nickel Alloy 800HT | UNS N08811 | 1.4959 | Incoloy 800HT

Nickel Alloy 800HT (UNS N08811 / 1.4959) is a nickel-iron-chromium alloy with tightly controlled Al+Ti content (0.85-1.20%) for maximum creep rupture strength above 700°C. Available in plate, sheet, round bar and tubing with EN 10204 3.1 certification.
Quality Nickel Alloy 825 | UNS N08825 | 2.4858 | Incoloy 825 factory

Nickel Alloy 825 | UNS N08825 | 2.4858 | Incoloy 825

Nickel Alloy 825 (UNS N08825 / 2.4858) is a nickel-iron-chromium alloy with molybdenum, copper and titanium additions for excellent resistance to reducing and oxidizing acids. Available in plate, sheet, round bar and tubing with EN 10204 3.1 certification .
Quality Nickel Alloy 800H | UNS N08810 | 1.4876 | Incoloy 800H factory

Nickel Alloy 800H | UNS N08810 | 1.4876 | Incoloy 800H

Nickel Alloy 800H (UNS N08810 / 1.4876) is a nickel-iron-chromium alloy with controlled carbon content (0.05-0.10%) for enhanced creep and rupture strength above 600°C. Available in plate, sheet, round bar and tubing with EN 10204 3.1 certification .
Quality Nickel 200 vs Nickel 201: A Comprehensive Comparison factory

Nickel 200 vs Nickel 201: A Comprehensive Comparison

Nickel 200 and 201 are commercially pure wrought nickel grades with nearly identical properties. The key difference is carbon content: 200 has 0.15% max for service below 315°C, while 201 has 0.02% max for elevated-temperature applications above 315°C .
Quality Alloy 400 vs Alloy K-500: A Comprehensive Comparison factory

Alloy 400 vs Alloy K-500: A Comprehensive Comparison

Alloy 400 is a solid-solution nickel-copper alloy with excellent seawater and HF resistance. Alloy K-500 adds Al+Ti for precipitation hardening, achieving double the strength while maintaining corrosion resistance. Choose based on strength requirements.
Quality Nickel Alloy C-276 | UNS N10276 | 2.4819 | Hastelloy C-276 factory

Nickel Alloy C-276 | UNS N10276 | 2.4819 | Hastelloy C-276

Nickel Alloy C-276 (UNS N10276 / 2.4819) is a nickel-molybdenum-chromium-tungsten alloy offering exceptional resistance to pitting, crevice corrosion and stress-corrosion cracking. Available in plate, sheet, round bar and tubing with EN 10204 3.1 certification.
Quality ASTM B409 Alloy 800H Plate | UNS N08810 | Incoloy 800H factory

ASTM B409 Alloy 800H Plate | UNS N08810 | Incoloy 800H

ASTM B409 Alloy 800H plate (UNS N08810 / 1.4876) is a nickel-iron-chromium alloy with controlled carbon content for enhanced creep-rupture strength above 600°C. Available in annealed condition with EN 10204 3.1 certification.
2 3 4 5 6 Next