| Attribute | Value |
|---|---|
| Material Type | Nickel-based Superalloy |
| Density | ~8.4 g/cm³ |
| Tensile Strength | ~750 MPa |
| Yield Strength | ~600 MPa |
| Temperature Range | Up to 1100°C (2012°F) |
| Oxidation Resistance | Excellent |
| Corrosion Resistance | Good |
| Applications | Aerospace, industrial gas turbines, exhaust systems |
| Heat Treatment | Solution treated and aged |
| Form | Bars, sheets, forgings, and custom shapes |
GH600 Alloy is a high-performance nickel-based superalloy specifically designed for applications requiring exceptional strength and durability at high temperatures. It provides outstanding mechanical properties, thermal stability, and oxidation resistance, making it ideal for severe environments.
GH600 Alloy's advanced properties make it suitable for demanding aerospace and industrial applications, ensuring long-term performance and reliability in challenging environments.
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 14.0 - 16.0 |
| Molybdenum (Mo) | 4.0 - 5.0 |
| Titanium (Ti) | 1.8 - 2.5 |
| Aluminum (Al) | 1.0 - 1.5 |
| Iron (Fe) | ≤ 4.0 |
| Carbon (C) | ≤ 0.08 |
| Silicon (Si) | ≤ 0.50 |
| Manganese (Mn) | ≤ 0.50 |
| Boron (B) | ≤ 0.01 |