Home ProductsNickel Based Alloys

GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength

Customer Reviews
We have been working with this factory for many years and everything has been going great. I love this factory!

—— Tony Hilton - Poland

Their ability to source rare specialty alloys with short lead times has been crucial for our oil and gas projects. Their global partnerships with premier steel mills ensure we get authentic materials with complete traceability.

—— Mohammed Al-FarsiGulf Energy

I have been looking for this supplier to cooperate with. The quality of their materials is very reliable and they are easy to communicate with.

—— Mahamoud Abid Iqbal

I'm Online Chat Now

GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength

GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength
GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength

Large Image :  GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength

Product Details:
Place of Origin: China
Brand Name: Zhonggong Special Metallurgy
Certification: ISO Certificate
Model Number: GH2132 alloy
Payment & Shipping Terms:
Minimum Order Quantity: 100KG
Price: Price is negotiated based on the required specifications and quantity
Packaging Details: Standard export packaging, or packaging as required
Delivery Time: 5-8 working days, depending on the parameters required for negotiation
Payment Terms: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability: 5000 tons per month

GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength

Description
Composition: Nickel-based Superalloy Containing Nickel, Chromium, Molybdenum, And Niobium Density: 8.4 G/cm³
Melting Point: 1290-1350°C (2354-2462°F) Tensile Strength: 760-1035 MPa (at Room Temperature)
Yield Strength (0.2% Offset): 350-765 MPa Elongation: 30-40%
Thermal Conductivity: 8.4 W/m·K (at 100°C) Specific Heat Capacity: 434 J/kg·K (at 20°C)
Coefficient Of Thermal Expansion: 12.8 µm/m·K (20-100°C) Electrical Resistivity: 1.34 µΩ·m (at 20°C)
Hardness: HRB 100 (max)
Highlight:

Nickel Alloy Rod Corrosion Resistance

,

Nickel Alloy Rod 8.4 g/cm3

GH2132 Alloy Nickel Alloy Rod 8.4 g/cm³ Corrosion Resistance High Strength
Product Attributes
Attribute Value
Composition Nickel-based superalloy containing Nickel, Chromium, Molybdenum, and Niobium
Density 8.4 g/cm³
Melting Point 1290-1350°C (2354-2462°F)
Tensile Strength 760-1035 MPa (at room temperature)
Yield Strength (0.2% offset) 350-765 MPa
Elongation 30-40%
Thermal Conductivity 8.4 W/m·K (at 100°C)
Specific Heat Capacity 434 J/kg·K (at 20°C)
Coefficient of Thermal Expansion 12.8 µm/m·K (20-100°C)
Electrical Resistivity 1.34 µΩ·m (at 20°C)
Hardness HRB 100 (max)
Product Description

GH2132 alloy, also known as Inconel 625, is a versatile nickel-based superalloy recognized for its exceptional combination of strength, toughness, and corrosion resistance. It maintains high tensile and yield strength across a broad temperature range, from cryogenic temperatures to over 1000°C (1800°F).

Key Features
  • Corrosion Resistance: Outstanding resistance to a wide range of corrosive environments, including seawater, acids, and alkalis.
  • High Strength: Excellent mechanical properties with high tensile and yield strength even at elevated temperatures.
  • Weldability: Easily weldable using conventional methods without significant loss in strength or corrosion resistance.
  • Fatigue Resistance: Exceptional fatigue and thermal-fatigue resistance for cyclic loading applications.
  • Applications: Aerospace, marine, and chemical processing industries for turbine blades, seals, and chemical processing equipment.
  • Machinability: Can be machined using conventional methods with appropriate tooling.
  • Heat Treatment: Can be annealed to restore desired properties after fabrication or welding.

GH2132 alloy (Inconel 625) is a preferred choice for demanding applications where resistance to corrosion, high temperatures, and mechanical stresses are essential.

Typical Composition
Element Composition (%)
Nickel (Ni) 58.0 min
Chromium (Cr) 20.0 - 23.0
Molybdenum (Mo) 8.0 - 10.0
Iron (Fe) 5.0 max
Niobium (Nb) 3.15 - 4.15
Cobalt (Co) 1.0 max
Manganese (Mn) 0.50 max
Silicon (Si) 0.50 max
Phosphorus (P) 0.015 max
Sulfur (S) 0.015 max
Carbon (C) 0.10 max
GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength 0 GH2132 Alloy Nickel Alloy Rod 8.4 g/cm3 Corrosion Resistance High Strength 1

Contact Details
Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.

Contact Person: John zhou

Tel: +8613306184668

Fax: 86-510-88232386

Send your inquiry directly to us (0 / 3000)