Product Details:
|
Nickel (Ni): | Balance | Chromium (Cr): | 20.0-22.0% |
---|---|---|---|
Iron (Fe): | 5.0-7.0% | Cobalt (Co): | 1.0-2.0% |
Density: | ~8.4 G/cm³ | Melting Point: | ~1370°C (2500°F) |
Thermal Conductivity: | ~10-12 W/m·K | Yield Strength: | ~690 MPa (100 Ksi) |
Ultimate Tensile Strength: | ~880 MPa (128 Ksi) | Elongation: | ~15% |
Highlight: | GH3044 Ni Based Superalloy,Ni Based Superalloy Oxidation Resistance |
GH3044 Alloy is a high-performance nickel-based superalloy designed for exceptional strength and oxidation resistance in high-temperature environments. This alloy is predominantly used in the aerospace and power generation industries due to its superior mechanical properties and resistance to extreme conditions.
GH3044 alloy's unique combination of strength, temperature resistance, and corrosion resistance makes it a preferred choice for demanding engineering applications, contributing to enhanced performance and extended service life of components.
Element | Content Range |
---|---|
Nickel (Ni) | Balance |
Chromium (Cr) | 20.0-22.0% |
Iron (Fe) | 5.0-7.0% |
Molybdenum (Mo) | 4.0-5.0% |
Tungsten (W) | 0.5-1.5% |
Cobalt (Co) | 1.0-2.0% |
Aluminum (Al) | 0.8-1.2% |
Titanium (Ti) | 1.0-2.0% |
Boron (B) | 0.005-0.015% |
Attribute | Value |
---|---|
Density | ~8.4 g/cm³ |
Melting Point | ~1370°C (2500°F) |
Thermal Conductivity | ~10-12 W/m·K |
Yield Strength | ~690 MPa (100 ksi) |
Ultimate Tensile Strength | ~880 MPa (128 ksi) |
Elongation | ~15% |
Contact Person: John zhou
Tel: +8613306184668
Fax: 86-510-88232386