| Attribute | Value |
|---|---|
| Material Type | Nickel-based Superalloy |
| Density | ~8.3 g/cm³ |
| Tensile Strength | ~850 MPa |
| Yield Strength | ~700 MPa |
| Temperature Range | Up to 950°C (1742°F) |
| Oxidation Resistance | Excellent |
| Corrosion Resistance | Good |
| Applications | Aerospace, power generation, chemical processing |
| Heat Treatment | Solution treated and aged |
GH333 Alloy is a high-performance nickel-based superalloy engineered for demanding high-temperature applications. It is designed to deliver exceptional strength, durability, and resistance to harsh environments, making it suitable for critical components in aerospace and industrial sectors.
GH333 Alloy's advanced properties make it an ideal choice for applications requiring high performance, resistance to extreme temperatures, and reliable long-term operation. Its robust nature ensures dependable service in some of the most challenging industrial and aerospace environments.
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 14.0 - 16.0 |
| Molybdenum (Mo) | 3.0 - 4.0 |
| Titanium (Ti) | 1.0 - 2.0 |
| Aluminum (Al) | 0.8 - 1.2 |
| Iron (Fe) | ≤ 4.0 |
| Carbon (C) | ≤ 0.08 |
| Silicon (Si) | ≤ 0.50 |
| Manganese (Mn) | ≤ 0.50 |
| Boron (B) | ≤ 0.01 |
These values are approximate and can vary slightly based on the specific production standards and requirements of the alloy.