| Density | 8.14 g/cm³ |
| Melting Range | 1280-1345°C |
| Tensile Strength | Up to 1380 MPa (200 ksi) at room temperature |
| Yield Strength | 1000 MPa (145 ksi) at room temperature |
| Elongation | 20-30% |
| Hardness (HB) | 277-302 HB |
| Thermal Conductivity | 10.3 W/m·K at 100°C |
| Coefficient of Thermal Expansion | 13.6 µm/m·K (20-100°C) |
| Electrical Resistivity | 1.12 µΩ·m at 20°C |
| Modulus of Elasticity | 196 GPa (28.4 x 10^6 psi) |
| Magnetic Properties | Non-magnetic |
| Element | Percentage Range |
|---|---|
| Nickel (Ni) | 42-46% |
| Iron (Fe) | 33-38% |
| Chromium (Cr) | 11-14% |
| Titanium (Ti) | 2.6-3.4% |
| Aluminum (Al) | 0.35-0.75% |
| Manganese (Mn) | 0.0-0.35% |
| Silicon (Si) | 0.0-0.4% |
| Sulfur (S) | 0.0-0.02% |
| Copper (Cu) | 0.0-0.2% |
| Carbon (C) | 0.0-0.1% |
| Cobalt (Co) | 0.0-0.1% |
| Phosphorus (P) | 0.0-0.015% |