| Attribute | Value |
|---|---|
| Density | ~8.3 g/cm³ |
| Melting Point | ~1400°C (2550°F) |
| Thermal Conductivity | ~11-13 W/m·K |
| Yield Strength | ~850 MPa (123 ksi) |
| Ultimate Tensile Strength | ~1000 MPa (145 ksi) |
| Elongation | ~12% |
| Hardness (Rockwell) | ~HRB 95-100 |
| Applications | Aerospace components, gas turbines, and high-temperature engines |
GH4169 Alloy is a high-performance nickel-based superalloy specifically designed for excellent strength and stability at elevated temperatures. It is widely used in demanding applications requiring exceptional thermal and oxidative resistance.
GH4169's combination of high strength, thermal stability, and corrosion resistance makes it an ideal choice for applications requiring reliable performance under severe conditions.
| Element | Content Range |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 19.0-21.0% |
| Iron (Fe) | 16.0-18.0% |
| Cobalt (Co) | 8.0-10.0% |
| Molybdenum (Mo) | 2.5-3.0% |
| Titanium (Ti) | 1.8-2.2% |
| Aluminum (Al) | 1.0-1.5% |
| Boron (B) | 0.005-0.015% |