| MOQ: | 100KG |
| Price: | Price is negotiated based on the required specifications and quantity |
| Standard Packaging: | Standard export packaging, or packaging as required |
| Delivery Period: | 5-8 working days, depending on the parameters required for negotiation |
| Payment Method: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Capacity: | 5000 tons per month |
| Attribute | Value |
|---|---|
| Density | ~8.3 g/cm³ |
| Melting Point | ~1390°C (2530°F) |
| Thermal Conductivity | ~11-12 W/m·K |
| Yield Strength | ~700 MPa (102 ksi) |
| Tensile Strength | 900 MPa (130 ksi) |
| Elongation | ~10% |
| Hardness (Rockwell) | ~HRB 90-95 |
| Applications | Aerospace components, gas turbines, and high-temperature industrial parts |
| Element | Content Range |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 18.0-21.0% |
| Iron (Fe) | 14.0-17.0% |
| Cobalt (Co) | 8.0-10.0% |
| Molybdenum (Mo) | 2.0-3.0% |
| Titanium (Ti) | 1.5-2.5% |
| Aluminum (Al) | 1.0-1.5% |
| Boron (B) | 0.005-0.015% |