| MOQ: | 100KG |
| Price: | Price is negotiated based on the required specifications and quantity |
| Standard Packaging: | Standard export packaging, or packaging as required |
| Delivery Period: | 5-8 working days, depending on the parameters required for negotiation |
| Payment Method: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Capacity: | 5000 tons per month |
| Attribute | Value |
|---|---|
| Density | ~8.9 g/cm³ (0.321 lb/in³) |
| Melting Point | ~1350-1450°C (2460-2640°F) |
| Tensile Strength | ~850 MPa (123 ksi) |
| Yield Strength | ~700 MPa (102 ksi) |
| Elongation | ~15% |
| Thermal Conductivity | ~14 W/m·K (8.4 BTU·in/hr·ft²·°F) |
| Modulus of Elasticity | ~210 GPa (30 x 10³ ksi) |
| Corrosion Resistance | Good oxidation and corrosion resistance at high temperatures |
| Applications | Aerospace, gas turbines, and high-temperature structural components |
GH36 Alloy is a high-performance nickel-based superalloy renowned for its exceptional mechanical properties and resistance to high-temperature environments. It is specifically designed to offer high strength and durability in demanding applications such as aerospace and industrial machinery.
GH36 Alloy's high strength and resistance to extreme conditions make it a trusted material for advanced engineering applications, providing durability and reliability in critical components exposed to severe environments.
| Element | Composition Range (%) |
|---|---|
| Nickel (Ni) | 60.0 - 65.0 |
| Chromium (Cr) | 15.0 - 20.0 |
| Cobalt (Co) | 5.0 - 10.0 |
| Molybdenum (Mo) | 2.0 - 4.0 |
| Iron (Fe) | ≤ 6.0 |
| Titanium (Ti) | 1.0 - 2.0 |
| Aluminum (Al) | 1.0 - 2.0 |
| Carbon (C) | ≤ 0.10 |
| Manganese (Mn) | ≤ 0.5 |
| Silicon (Si) | ≤ 0.5 |
| Sulfur (S) | ≤ 0.01 |
These values provide general guidelines. For precise specifications or detailed applications, consult specific standards or suppliers.